Most gold deposits occur associated with sulphides like pyrite and arsenopyrite; thus, precious metal dissolution is possible by oxidizing auriferous sulfide concentrate using simultaneous pressure oxidation and cyanidation. The effectiveness of this process of extraction can be influenced by the temperature, cyanide (NaCN) concentration, and oxygen pressure. In this study, we conducted experiments to characterize the effects on gold extraction of ores using a range of sodium cyanide concentrations (1–8 g/L), temperatures (40–75 °C), and oxygen pressures (0.5–1.1 MPa). Characterization of the ores showed that pyrite and quartz were the main minerals present in the concentrate. The best results in terms of the highest extraction of Au were obtained with an oxygen pressure of 0.5 MPa, 6 g/L sodium cyanide, and a temperature of 75 °C, along with a constant stirring speed of 600 rpm. These conditions allowed for approximately 95% gold extraction in 90 min.

Idioma originalInglés
Número de artículo116
PublicaciónMinerals
Volumen13
N.º1
DOI
EstadoPublicada - ene. 2023

Nota bibliográfica

Publisher Copyright:
© 2023 by the authors.

Huella

Profundice en los temas de investigación de 'Gold Extraction from a Refractory Sulfide Concentrate by Simultaneous Pressure Leaching/Oxidation'. En conjunto forman una huella única.

Citar esto