New route for the synthesis of ammonia-free CdS tetrapods nanoparticles at room temperature by chemical bath deposition

S. J. Castillo, A. Apolinar-Iribe*, R. Ochoa-Landín

*Autor correspondiente de este trabajo

Producción científica: Contribución a una revistaArtículorevisión exhaustiva

Resumen

At this work, it is presented a new route to produce ammonia-free cadmium sulfide tetrapod nanoparticles at room temperature using three precursors, cadmium nitrate, polyethyleneimine and thioacetamide by chemical bath deposition method. The tetrapod cadmium sulfide nanoparticles were characterized by UV-Vis spectrum, transmission electronic microscope and Raman analysis. The optical band gap of tetrapod nanoparticles was 2.78 eV, the length of the arms was 39.45 nm and its width was 3.27 nm. From TEM was found an orthorhombic crystallographic structure of the nanoparticles and vibration modes (1LO = 272.79 nm and 1LO = 292.79 nm).

Idioma originalInglés
Páginas (desde-hasta)591-594
Número de páginas4
PublicaciónDigest Journal of Nanomaterials and Biostructures
Volumen13
N.º2
EstadoPublicada - 1 abr. 2018

Nota bibliográfica

Publisher Copyright:
© 2018, S.C. Virtual Company of Phisics S.R.L. All rights reserved.

Huella

Profundice en los temas de investigación de 'New route for the synthesis of ammonia-free CdS tetrapods nanoparticles at room temperature by chemical bath deposition'. En conjunto forman una huella única.

Citar esto